Ores of reactive metals have to be heated with carbon or carbon monoxide in order to extract the metal. Copper oxide powder is mixed with carbon powder. The mixture is heated strongly for a few ...
THE measurement of the electrical resistance of films of copper oxide on copper showing interference colours of the first order has given results varying from 0.002 to 15 ohms per sq. cm.